Design Of Environmentally Friendly Fiberglass Compositions: Ternary Eutectic Sio2-Al2O3-Cao Compositions, Structures And Properties

Incumbent E-glass compositions, which are used for the manufacture of reinforcing fibres for structural composites (eg in automotive applications) and for electronic laminates, contain 6-8% B2O3 and 0.1-1.0% fluorine. B2O3 and fluorine can cause hazardous particulate and toxic vapour emissions during manufacture. New, environmentally friendly E-glass compositions, which are beginning to replace these compositions in structural applications are fluorine-free and contain either no B2O3, or only small amounts of B2O3. This paper deals with the design of ternary, boron-and fluorine-free fiberglass compositions which have the lowest possible log3 fibre forming temperature in the ternary SiO2-Al2O3-CaO system, would be suitable for use in a continuous commercial melt and fibre forming process and would require the lowest possible process energy.

Author
F T Wallenberger Et Al
Origin
Ppg Inc, Usa
Journal Title
J Non-Cryst Solids 349 2004 377-387
Sector
Glass Fibre
Class
GF 464

Request article (free for British Glass members)

Design Of Environmentally Friendly Fiberglass Compositions: Ternary Eutectic Sio2-Al2O3-Cao Compositions, Structures And Properties
J Non-Cryst Solids 349 2004 377-387
GF 464
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.