Dependence Of Properties On Structural Units In Li20-Al203-Si02 Glasses

Density, thermal expansion coefficient, transformation temperature and electrical resistivity have been investigated for (33-x) Li20.xAl203.67Si02 glasses.

Author
G El-Damrawi & H Doweidar
Origin
Mansoura University, Egypt
Journal Title
Phys Chem Glasses 42 2 2001 116-120