Dependence Of Emissivity On Angle For Coated And Uncoated Glass And The Calculation Of Radiant Energy Exchange In Double-Glazed Units

The angular dependence of emissivity has been calculated for glass coated in various ways, including some which simulate commercial coatings. The currently used factors have been shown to be satisfactory for commercial coatings used at present but may need to be revised as new coatings are introduced.