Density Of Ti02-Doped Vitreous Silica

The effect of composition on the density of titanium-doped vitreous silica has been reported by a number of investigators, with varying results. While it is widely believed that the density of these glasses is almost independent of composition, their are studies which contradict this finding. The current study discusses the density of as-received titanium-doped silicas containing from 0-10 mol% TiO2 and the effect of changes in fictive temperature on the density of these glasses. The effect of y-irradiation on the density of a commercial titanium-doped silica is also discussed. An expression for the relation between the position of the infrared band used to determine the fictive temperature of undoped vitreous silica and the TiO2 concentration of these glasses is derived from the data.

Author
J E Shelby
Origin
Alfred University, Usa
Journal Title
Phys Chem Glasses 46 5 2005 494-499
Sector
Special Glass
Class
S 3044

Request article (free for British Glass members)

Density Of Ti02-Doped Vitreous Silica
Phys Chem Glasses 46 5 2005 494-499
S 3044
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.