Density, Surface Tension And Viscosity Of Pbo-B203-Si02 Glass Melts

The density, surface tension, & viscosity of the melts from the PbO-B2O3-SiO2 system have been measured at temperatures in the range 1073-1473K. The effect of composition on these properties was also investigated. Density of the melt was found to increase linearly with increasing PbO content. Molar volume was derived from the density data, & its deviation from the additivity of partial molar volumes was calculated. These deviations in molar volume from those obtained from additivity rules have been used along with the ratio of various coordination numbers of boron (as reported by Bray) to discuss the structure of the melts. The surface tension was found to decrease with decreasing SiO2/B2O3 ratio, & to increase in the range of the PbO content between 30-60 mol%, showing a maximum at ~60 mol% PbO, & then decreased with further additions.

Author
S Fujino Et Al
Origin
Kyushu University, Japan
Journal Title
J Am Ceram Soc 87 1 2004 10-16
Sector
Special Glass
Class
S 2675

Request article (free for British Glass members)

Density, Surface Tension And Viscosity Of Pbo-B203-Si02 Glass Melts
J Am Ceram Soc 87 1 2004 10-16
S 2675
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.