Density Of Quarternary Glassses In The Mgo-Cao-Al2O3-Sio2-System - Modeling Vs Measurement

The densities of quarternary glass-forming systems within the MgO-CaO-AL2O3-SiO2-composition (CMAS) were evaluated. Their compositions differed not more than 5mol% for each component from each other. After melting, the exact chemical compositions were measured using RF and the densities were determined by Archimedes method and pycnometry. This property and its dependency upon small variations in the composition is the main focus of this paper.

Author
U Veit & C Russel
Origin
Otto-Schott Inst, Jena, Germany
Journal Title
Appl Glass Sci 8 2017 301-312
Sector
Special Glass
Class
S 4411

Request article (free for British Glass members)

Density Of Quarternary Glassses In The Mgo-Cao-Al2O3-Sio2-System - Modeling Vs Measurement
Appl Glass Sci 8 2017 301-312
S 4411
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.