Abstract Glasses with composition (ZnO)30(MgO)x (P2O5)70-x (x = 5, 8, 10, 13, 15, 18, and 20 mol.%) have been successfully prepared by the melt-quenching technique. Degradation study has been carried out by means of measuring their chemical durability against buffer solutions with initial pH values of 4.01, 7.00, and 10.01 at an ambient temperature for up to 30 days. The dissolution rate (DR) was obtained by calculating the measured weight loss of the glasses per unit surface area per unit immersion time. The results show that the glasses have better corrosion resistance in basic solution. It was also found that the weight loss is related to the MgO concentration with lower P2O5 concentration exhibiting greater corrosion resistance irrespective of acidic, neutral, or basic solutions as immersion liquid. All the sample surfaces and edges were corroded and the solutions experienced a decrease in pH values during the duration of the corrosion test.

Author
S F Khor Et Al
Origin
Unknown
Journal Title
J Materials Science 46 Dec 2011 7895–7900
Sector
Special Glass
Class
S 4211

Request article (free for British Glass members)

Degradation Study On Ternary Zinc Magnesium Phosphate Glasses
J Materials Science 46 Dec 2011 7895–7900
S 4211
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.