Degradation Of Commercial Window Glass

Corrosion of commercial soda-lime-silica window glass specimens in the presence of water has been investigated. The aims are: (i) to elucidate the degradation mechanism involved when glass sheets are stored in blocks in humid environment, and; (ii) the time required to reach the stage when individual sheets could not be separated from each other. Results of experimental work confirm the generally accepted theory that dealkalisation of the glass surface precedes the breakdown of the silica structure.

Author
R Wurher & A Ray
Origin
University Of Technology, Sydney
Journal Title
Key Eng Materials V53-55 372-376 1991
Sector
Flat glass
Class
F 443

Request article (free for British Glass members)

Degradation Of Commercial Window Glass
Key Eng Materials V53-55 372-376 1991
F 443
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.