Deforamtion Of Fluid Inclusions In Glass Melts. Part 2: Effect Of Interfacial Tension

Part 1 examined theoretical models for the deformation of miscible inclusions of viscosity different from their surroundings and deformation was shown to depend on total shear. The effect of inter facial tension on the deformation of the immiscible spherical inclusions is examined here.