Decrease Of Mechanical Properties Of Glass Or Carbon Fibres Reinforced Pei In Several Chemical Environments

This work shows how the mechanical properties, tensile and shear strength, are modified in different ways if two different types of composite materials are immersed in toluen and sulfuric acid. The composites have a thermoplastic as matrix, one of these reiforced with glass fibre, the other with carbon fibre.

Author
J Vina Et Al
Origin
Ets Ingenieros Industriales
Journal Title
Bol Soc Esp Ceram Vidrio 39 4 2000 511-513
Sector
Glass Fibre
Class
GF 249

Request article (free for British Glass members)

Decrease Of Mechanical Properties Of Glass Or Carbon Fibres Reinforced Pei In Several Chemical Environments
Bol Soc Esp Ceram Vidrio 39 4 2000 511-513
GF 249