Decoration And Annealing Of Bottles And Vials

This article described technical elements associated with Cobelcomex's decorating lehr technology, covering colours and metals, geometry, laws of heat transfer, thermal cycles and radiation absorption.

Author
G Coudamy, G Angely
Origin
Cobelcomex
Journal Title
Glass Machinery Plants & Accessories 5 6 1992 50-51