Decorating Techniques Of Treated Glass Containers

Just as there are various formulations of glass to suit specific applications, so there are various decorating options. This paper looks at different decorating techniques and their implications.

Author
L Pulcano
Origin
Algroup Wheaton, Usa
Journal Title
Glass 77 6 July 2000 186-187
Sector
Container glass
Class
C 1601

Request article (free for British Glass members)

Decorating Techniques Of Treated Glass Containers
Glass 77 6 July 2000 186-187