Dc And Ac Electrical Conductivity Of Rare Earths Doped Tellurite Glasses

Binary Te02 glasses with different rare earth modifiers have been prepared in the form of [Te02-RE] where RE is 10 mol% (La203, Ce02, Pr203, Nd203, Sm203 and Yb203). The dc and ac electrical conductivity of each glass has been measured over the temperature range 80-500K. The dc conductivity is described at high temperatures by the well known Arrhenius relation. As the temperature is lowered, the multiphonon processes are frozen out and the high temperature activation energy is expected to drop continuously. During incorporation of rare earth oxides an oxidation-reduction mechanism may be taking place.

Author
M M Elkholy
Origin
Menoufa University, Egypt
Journal Title
Phys Chem Glasses 42 1 2001 49-55
Sector
Special Glass
Class
S 2152

Request article (free for British Glass members)

Dc And Ac Electrical Conductivity Of Rare Earths Doped Tellurite Glasses
Phys Chem Glasses 42 1 2001 49-55
S 2152
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.