The Association of the Glass and Ceramics Industry of the Czech Republic, in collaboration with the Ministry of Industry and Trade of the Czech Repoublic, the Czech Glass Society and MM Consult Prague has prepared the second edition of its annual report. This survey details the performance of Czech manufacturers during 1995. It includes data from all companies operating in these sectors and draws comparisons from data gathered over the last five years.