Cylindrical Furnace For Continuous Production Of Reinforced And Nonreinforced Seamless Pipes Of Foam Glass.

Foam glass is poured into a vertical annular chamber of a furnace through a header which rotates about the chamber axis to deposit the glass as a helical layer. The temperature of the chamber is controlled to let the glass harden as it descends.