Cutting Performance Of Advanced Ceramic Tools

Four advanced ceramic cutting tools were used to machine the nickel-based super alloy Inconel 718 under various conditions.

Author
H Chuanzhen Et Al
Origin
Shandong University Of Technology, Pr China
Journal Title
Am Ceram Soc Bull 76 7 1997 83-85
Sector
Glass Ceramics
Class
GC 283

Request article (free for British Glass members)

Cutting Performance Of Advanced Ceramic Tools
Am Ceram Soc Bull 76 7 1997 83-85
GC 283