Current Understanding And Remaining Challenges In Modeling Long-Term Degradation Of Borosilicate Nuclear Waste Glasses

Chemical durability is not a single material property that can be uniquely measured. Instead, it is the response to a host of coupled material and environmental processes whose rates are estimated by a combination of theory, experiment and modeling. High-level nuclear waste (HLW) glass is perhaps the most studied of any material, yet there remain significant technical gaps regarding their chemical durability. The phenomena affecting the long-term performance of HLW glasses in their disposal environment include surface reactions, transport properties to and from the reacting glass surface, and ion exchange between the solid glass and the surrounding solution and alteration products. The rates of these processes are strongly influenced and are coupled through the solution chemistry, which is in turn influenced by the reacting glass and also by reaction with the near-field materials and precipitation of alteration products. Therefore, those processes must be understood sufficiently well to estimate or bound the performance of HLW glass in its disposal environment over geologic time scales. This article summarises the current state of understanding of surface reactions, transport properties and ion exchange along with the near-field materials and alteration products influences on solution chemistry and glass reaction rates. Also summarised are the remaining technical gaps along with recommended approaches to fill those technical gaps.

Author
J D Vienna Et Al
Origin
Pacific Northwest National Labs, Washington, Usa
Journal Title
Int J Appl Glass Sci 4 4 2013 283-294
Sector
Special Glass
Class
S 4067

Request article (free for British Glass members)

Current Understanding And Remaining Challenges In Modeling Long-Term Degradation Of Borosilicate Nuclear Waste Glasses
Int J Appl Glass Sci 4 4 2013 283-294
S 4067
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.