The Cuprous-Cupric Redox Equilibrium In Binary Alkali Silicate Glasses

An equation to represent the Cu+ - Cu2+ redox equilibrium is suggested following a critical examination of earlier models and a study of binary alkali silicate glasses in air at 1400C.

Author
S P Singh, A Kumar
Origin
Banaras Hindu University, Varanasi, India
Journal Title
Physics & Chemistry Of Glasses 34 2 2 1993 45-51