Cullet is one of the most important raw materials in glass melting. The condition of the cullet used has a significant effect on the quality and characteristics of the glass produced. The use of cullet offers advantages in glass melting, hence, correct handling and suitable treatment equipment help produce high quality factory and foreign cullet.

Author
J Rosenthal
Origin
Eme Gmbh, Germany
Journal Title
Int Glass Journal 96 July-Sept 1998 46-50
Sector
Container glass
Class
C 1240