Cullet In Amber Glass Production

Glassworks experience in the use of cullet levels up to 80% and the use of flint/green cullet in amber glass is discussed. The effects on the resulting glass properties are examined.

Author
C Baltazar-Brillante
Origin
San Miguel Corporation
Journal Title
Glass Machinery Plants & Accessories 1989 2 6 47-51
Sector
Container glass
Class
C 290