Crystallization Of Titanosilicate Glasses For Nuclear Waste Immobilization

The effects of different cooling and reheating rates on the phase constitutions of Na2O-Al2O3-TiO2-SiO2 glass-ceramics containing up to 20 wt% of simulated nuclear fuel recycle waste have been studied using X-ray diffraction, differential thermal analysis, and scanning and transmission electron microscopy.