Crystallization Kinetics Of Tellurite Glasses Studied By Dsc And Dta

Crystallization kinetics of two tellurite glasses were studied using isothermal and non-isothermal methods. DSC and DTA scans were employed to obtain respectively isothermal and non-isothermal data. A binary and a ternary tellurite glass compositions were studied and compared. Crystallization kinetics were analyzed using the Johnson-Mehl-Avrami theory, and crystal growth parameters were obtained. Time-temperature-transformation curves were calculated.

Author
S Shen Et Al
Origin
University Of Leeds, Uk
Journal Title
Glastech Ber Glass Sci & Technol 73 C1 2000 111-119
Sector
Special Glass
Class
S 3841

Request article (free for British Glass members)

Crystallization Kinetics Of Tellurite Glasses Studied By Dsc And Dta
Glastech Ber Glass Sci & Technol 73 C1 2000 111-119
S 3841
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.