Crystallization Behaviour Of Potassium Niobium Silicate Glasses

Crystallization behaviour of potassium niobium silicate (KNS) glasses having compositions expressed by the general formula xK20.xNb205.(1-2x)Si02, with x=0.167, 0.182, 0.200, 0.220, and 0.250, has been studied by DTA, X-ray diffraction, second harmonic optical generation (SHG), and electron microscopy.