Crystallization Behaviour Of 45S5 Bioactive Glass Modified By Therapeutic Ions

This is the first study that investigates the crystallization behaviour of strontium and copper-doped bioactive glasses by both isothermal and non-isothermal methods using differential thermal analysis (DTA) data. DTA results showed that bioactive glasses are suitable for glass-ceramics production. Isothermal and isothermal DTA experiments indicated that the crystallisation activation energies of strontium-doped bioactive glasses are in the range of 304.1-327.7 kJ/mol, whereas the activation energies of copper-doped bioactive glasses change in the range of 219.13-263.20kJ/mol. It was found that crystallisation activation energies of strontium-doped glasses are higher than those of the copper-doped glasses. Results revealed that isothermal and non-isothermal crystallisation kinetics of strontium and copper-doped bioactive glasses are in agreement within the experimental error.

Author
M E Taygun And V Hocaoglu
Origin
Technical University Maslak, Turkey
Journal Title
Int J Appl Glass Sci 9 1 2018 62-69
Sector
Special Glass
Class
S 4449

Request article (free for British Glass members)

Crystallization Behaviour Of 45S5 Bioactive Glass Modified By Therapeutic Ions
Int J Appl Glass Sci 9 1 2018 62-69
S 4449
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.