Crystallization Of Barium Osumilite Glass

The crystallization of stoichiometric barium osumilite (BaMg2Al6Si9O30) glass manufactured by melting or by sol-gel processing using an all-alkoxide route (AAR) or a partial-alkoxide route (PAR) using mixed alkoxides and salts has been characterized by thermal methods, phase analysis, and microstructural analysis.