Crystallisation Of Teo2-Zncl2-Pbcl2 Glass System

A series of infrared transmitting glasses based on TeO2-ZnCl2-PbCl2 system has been prepared. The thermal properties and crystallisation behaviour of the system have been studied by DTA, XRD, EDX, IR spectroscopy and electron microscopy Tc-Tg gaps up to 84 degrees can be achieved. It is observed that the predominant crystal phases that occured on crystallised glass are TeO2, MTeO3 and TeOCl2. Growth rates are reported for the glasses and these can be observed to be strongly dependent on the chlorine content.

Author
M R Sahar Et Al
Origin
University Technology Of Malaysia
Journal Title
Proc Of Xvi Icg, Beijing, China Vol7 1995 54-59
Sector
Special Glass
Class
S 1470

Request article (free for British Glass members)

Crystallisation Of Teo2-Zncl2-Pbcl2 Glass System
Proc Of Xvi Icg, Beijing, China Vol7 1995 54-59
S 1470
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.