Crystallisation Of A Lead Borate Glass And Its Influence On The Thermoluminescence Response

Lead borate glasses of the composition 33PbO.67B2O3 were prepared by the conventional melting/quenching method. Glass-ceramics were prepared from powdered glasses by heat treatment at 590 deg C for 60, 120, 180 and 240 minutes. The crystallisation process was followed by scanning electron microscopy. The thermoluminescence of the glasses and glass-ceramics was measured and the response was correlated with the structural changes that occur during crystallisation. A great improvement in the thermoluminescence response was obtained after 60 minutes of isothermal crystallisation, which corresponds to a degree of crystallisation of more than 50%. As the crystallisation proceeds the glass structure changes and a localised state which improves the response of the materials is generated. These results indicate that the studied lead borate glass-ceramics are promising materials for thermoluminescence dosimetric applications.

Author
M R Chinlanza Et Al
Origin
University Repoublic Montevidro, Uruguay
Journal Title
Phys Chem Glasses 54 6 2013 241-246
Sector
Special Glass
Class
S 4086

Request article (free for British Glass members)

Crystallisation Of A Lead Borate Glass And Its Influence On The Thermoluminescence Response
Phys Chem Glasses 54 6 2013 241-246
S 4086
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.