Crystallisation Kinetics Of Substituted Inf3 Glass By Differential Scanning Calorimetry

The kinetics of crystallisaiton in the substituted InF3 glass with good infrared transmission was studied by isothermal and nonisothermal methods using differential scanning calorimetry.