Crystallisation Of Doped Chalcogenide Glasses

The aim of this research was to produce infrared transmitting chalcogenide glass-ceramics, nucleated by appropriated nucleants. These materials, transparent in a wide range of the IR region, with improved thermal and mechanical properties are to be applied as passive or active components in high-power lasers and solar energy applications.

Author
L Boehm And H Assaf
Origin
Soreq Nuclear Research Centre, Yavne, Israel
Journal Title
Icg Madrid 2 1992 97-102
Sector
Special Glass
Class