Crystallisation Behaviour, Microstructure And Magnetic Properties Of Bao-Fe203-B2O3-Si02 Glass Ceramics

Differential thermal analysis, X-ray diffractometry and scanning electron microscopy with energy dispersive spectroscopy were used to study the crystallisation of glass ribbons with a composition of 35% BaO, 35% Fe2O3, 20% B2O3 and 10% SiO2 (mol%) prepared via cooling the melts between steel rollers. The magnetic properties of specimens were also measured with a vibrating sample magnetometer.

Author
M Mirkazemi Et Al
Origin
Iran University, Tehran
Journal Title
Ceramics International 32 2005 43-51
Sector
Glass Ceramics
Class
GC 643

Request article (free for British Glass members)

Crystallisation Behaviour, Microstructure And Magnetic Properties Of Bao-Fe203-B2O3-Si02 Glass Ceramics
Ceramics International 32 2005 43-51
GC 643
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.