The Crystallisation Of Barium Fluorozirconate Glasses Containing Lithium Fluoride

The devitrification products obtained on reheating barium fluorozirconate glasses containing lithium fluoride have been identified by powder X-ray diffraction analysis and electron probe microanalysis.