Crystallinity Analysis Of Glass-Ceramics By The Rietveld Method

The crystallinity of multicomponent glass-ceramic mixtures has been analyzed via the Rietveld method, using powder X-ray diffractormetry data. The Rietveld technique uses an internal standard but requires no calibration data to determine the total amorphous phase content of a mixture.