Crystal Structure Defects And Mechanical Strength In Crystalline Vitreous Materials (Russian)

It has been shown that the defect structure of alkali-free glass ceramics can be reduced, and their strength increased, by introducing two divalent cations, Ca and Ba, relative to those containing only one divalent cation.