Crystal Nucleation In Lithium Diborate Glass

The magnitude and temperature dependence of the nucleation rate were determined and compared with the predictions of classical nucleation theory.

Author
G L Smith, M C Weinberg
Origin
University Of Arizona
Journal Title
Phys Chem Glasses 1991 32 2 37-42
Sector
Special Glass
Class
S 523