A Crucible Salt Saturation Method For Determining Sulfur Solubility In Glass Melt

Experiments were conducted to determine sulfur solubility in Hanford low-activity waste (LAW) glass melts by a sulfur saturation method. Sulfur-incorporated glass melts were prepared by salt saturation and bubbling methods. The salt saturation method was performed by mixing crushed premelted baseline glasses with an excess amount of Na2SO4 prior to melting the mixture at 1150 deg C for 1 hour. The bubbling method involved bubbling the glass melt at 1150 deg C in a Pt crucible with a SO2/O2/N2 gas mix to equilibrate the melt at a known pressure of SO3. Preliminary results suggested that performing one cycle of mixing and melting was not sufficient to saturate the glass. The bubbling method successfully incorporated sulfur into the glass but caused significant losses of sodium from the melt. In order to saturate the glass melt with sulfate without causing noticeable sodium loss, a modified crucible salt saturation method was developed by repeating the mixing and melting of the glass and salt mixture. For all 3 representative LAW glasses tested in this study, it was found that after 3 mixing and melting cycles, the sulfur concentration reaches a plateau, indicating reasonable sulfur saturation.

Author
Un-named
Origin
Unknown
Journal Title
Int J Appl Glass Sci 10 1 January 2019 92-102
Sector
Special Glass
Class
S 4501

Request article (free for British Glass members)

A Crucible Salt Saturation Method For Determining Sulfur Solubility In Glass Melt
Int J Appl Glass Sci 10 1 January 2019 92-102
S 4501
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.