Creep Behaviour Of Soda-Lime Glass In The 100-500K Temperature Range By Indentation Creep Test

The loading time and temperature dependences viscoelastic behaviour of a soda-lime-silicate glass (SLS) were studied by indentation creep experiments. Experiments were conducted in air,water and silicone oil with 15-10,000s loading times, and temperatures ranging between 100 and 500K. The indentation size was found to depend much on the loading time and temperature. Hardness was found to decrease significantly with increasing loading time, even at 173K, and to decrease rapidly with rising temperature, even well below the glass transition temperature (Tg). Water on the surface of glasses appeared to reduce the hardness and indentation viscosity of the glass.

Author
H Shang & T Rouxel
Origin
University De Rennes, France
Journal Title
Jacs 88 9 2005 2625-2628
Sector
General
Class
G 3045

Request article (free for British Glass members)

Creep Behaviour Of Soda-Lime Glass In The 100-500K Temperature Range By Indentation Creep Test
Jacs 88 9 2005 2625-2628
G 3045
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 15 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.