Crack-Tip Structure In Soda-Lime-Silicate Glass

The topology of crack tips in soda-lime-silicate glass was investigated using atomic force microscopy (AFM). Studies were conducted on cracks that were first propagated in water and then subjected to stress intensity factors either at or below the crack growth threshold. Exposure to loads at the crack growth threshold resulted in long delays to restart crack growth after increasing the stress intensity factor to higher values. After breaking the fracture specimen in two, the "upper" and "lower" fracture surfaces were mapped and compared using AFM. Fracture surfaces matched to an accuracy of better than 0.5nm normal to the fracture plane and 5nm within the fracture plane. Displacements between the upper and lower fracture surfaces that developed after a critical holding time were independent of distance from the crack tip, & increased with holding time.

Author
J Guin Et Al
Origin
Nist, Usa
Journal Title
J Am Ceram Soc 88 3 2005 652-659
Sector
Special Glass
Class
S 2939

Request article (free for British Glass members)

Crack-Tip Structure In Soda-Lime-Silicate Glass
J Am Ceram Soc 88 3 2005 652-659
S 2939
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.