Crack Suppression In Strongly Bonded Homogeneous/Heterogeneous Laminates: A Study On Glass/Glass-Ceramic Bilayers

A study is made of glass/glass-ceramic bilayer as a model homogeneous/heterogenous laminate. The underlying objective is microstructural design of ceramic layer systems with optimum mechanical properties, alternating hard layers, for wear resistance, with tough layers for fracture resistance. Mica flakes in the glass-ceramic layer inhibit the propagation of well-developed intrusive cracks, by bridging; these same flakes render the structure susceptible to distributed damage, by providing a discrete weakness at the microstructural level.

Author
Un-named
Origin
S Wuttiphan Et Al
Journal Title
Materials Science & Eng Labs, Usa
Sector
Glass Ceramics
Class
GC 235

Request article (free for British Glass members)

Crack Suppression In Strongly Bonded Homogeneous/Heterogeneous Laminates: A Study On Glass/Glass-Ceramic Bilayers
Materials Science & Eng Labs, Usa
GC 235
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.