Coupled Modelling Of Redox Reactions & Glass Melt Fining Processes

The quality of glass depends upon the removal of dissolved gases and bubbles. A quantitative understanding of these processes is essential for glass production today, where quality requirements are becoming increasingly stringent. Classical fining involves adding an element or compound to the melt which will, through oxidation-reduction reactions at high temperatures, produce gases that diffuse into the bubbles present in the melt. The growth of these bubbles then enhances the rate of bubble removal from the melt. The modelling of oxidation-reduction reactions & that of fining are generally treated independently from one another. However, due to the large number of bubbles present, a significant amount of dissolved gases are consumed & the chemical equilibrium in the melt is changed.

Author
F Pigeonneau
Origin
Saint-Gobain Recherche, France
Journal Title
Glass Technology April 2007 Volume 48 2 66-72
Sector
Special Glass
Class
S 3293

Request article (free for British Glass members)

Coupled Modelling Of Redox Reactions & Glass Melt Fining Processes
Glass Technology April 2007 Volume 48 2 66-72
S 3293
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.