Corrosion Of Molybdenum Electrodes In Lead Glass Melts. Part 2. Effect Of Potential And Transfer Of Alternating Current By The Electrode

A comparison of the values of corrosion of molybdenum electrodes shows that the rest corrosion current is substantially lower than the mean value of alternating current over the current density range of 0.1 to 1 A/cm2 considered. The efficiency of hypothetical alternating-current electrolysis amounts to only 12 to 24 %. The alternating current is probably for the most part transferred by a reversible reaction. The dependence of corrosion rate of molybdenum in glass melts containing PbO on frequency exhibits a twin minimum whose frequencies decrease with the total content of alkalies while being independent of the Na2O:K2O ratio. The corrosion rate, separation of lead and the total current all exhibit a substantial increase when the potential is reduced by 200 to 300 mV compared to the rest potential, i.e. at -840 to -940 mV with respect to the oxygen electrode. Oxidation of Mo occurs even under these conditions. The separation of lead ceases when the potential is increased by 100 mV. The reaction of the molybdenum oxidation products with the alkalies in the glass melt probably plays a significant role in the entire corrosion process as well as in the alternating current transfer between the molybdenum electrode and the glass melt.

Author
J Matej Et Al
Origin
Inst Inorganic Chem Of Academy Of Sciences, Czech Republic
Journal Title
Ceramics 42 3 1998 132-140
Sector
General
Class
G 4160

Request article (free for British Glass members)

Corrosion Of Molybdenum Electrodes In Lead Glass Melts. Part 2. Effect Of Potential And Transfer Of Alternating Current By The Electrode
Ceramics 42 3 1998 132-140
G 4160
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.