Corrosion Of Bourre Glass Fibres In Borate Water Solution

BOURRE™ glass fibres are commonly used as thermal insulation in nuclear power plants. In the event of a loss of coolant accident (LOCA) these fibres can be strongly corroded by the coolant. The pH value of the coolant is stabilised by H3BO3/NaOH buffering systems. Therefore, the chemical durability of BOURRE fibres was tested in this work. Isothermal single pass flow-through leaching tests were conducted. In addition, recirculating tests were performed with the temperature profile of the leaching medium similar to that in post-LOCA thermal conditions. Glass dissolution was followed by inductively coupled plasma optical emission spectroscopy and the corroded surface of the glass fibre was studied by scanning electron microscopy and energy dispersive spectroscopy.

Author
V Soltesz Et Al
Origin
Vuez, Levice, Slovakia
Journal Title
Glass Technol 53 4 2012 139-145
Sector
Glass Fibre
Class
GF 713

Request article (free for British Glass members)

Corrosion Of Bourre Glass Fibres In Borate Water Solution
Glass Technol 53 4 2012 139-145
GF 713
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.