Corrosion Behaviour Of Some Selected Bioglasses By Different Aqueous Solutions

Corrosion studies of some selected bioglasses were carried out using the grain method. This investigation includes the study of the effect of varying the glass composition, leaching solution and duration of the immersion in the respective solution. Experimental results indicate that the weight loss changed depending on the type of oxide introduced. The effects of various factors were evaluated and correlated with the ability of the studied oxide to promote or retard the corrosion mechanism.

Author
K M El Badry Et Al
Origin
National Research Centre, Cairo
Journal Title
Glass Technol 43 4 Aug/02 162-170
Sector
Special Glass
Class
S 2613

Request article (free for British Glass members)

Corrosion Behaviour Of Some Selected Bioglasses By Different Aqueous Solutions
Glass Technol 43 4 Aug/02 162-170
S 2613
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.