Corrosion Behaviour Of Post-Deposition Polished Droplets-Embedded Arc Evaporated And Droplets-Free Hipims/Dcms Coatings

In this study, the effect of metal rich core of the droplets on the corrosion properties of TiN, CrN and ZrN arc evaporated nitride coatings has been investigated and the corrosion properties of such coatings have been compared with droplet free, highly dense coatings grown by combined high power impulse magnetron sputtering and direct current magnetron sputtering technique.

Author
Dr A A Sugumaran Et Al
Origin
Unknown
Journal Title
Corrosion January 2017: Shura.Shu.Ac.Uk/14594/
Sector
Special Glass
Class
S 4300

Request article (free for British Glass members)

Corrosion Behaviour Of Post-Deposition Polished Droplets-Embedded Arc Evaporated And Droplets-Free Hipims/Dcms Coatings
Corrosion January 2017: Shura.Shu.Ac.Uk/14594/
S 4300
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.