Correlation Of Properties Of Composite Materials Based On Siloxane Binder With The Type Of Filler

Composite ceramic materials are produced by the sol-gel method, based on siloxane binder and finely disperse powders of high-melting fillers (based on various borides, nitrides, and carbides which do not require lengthy sintering at hight temperatures. It is established that the best filler is AIN, and after heat treatment at 900c material based on this filler shows increased hardness, strength, and heat stability.

Author
I M Yao Etal
Origin
State Technological University, Kazan, Russia
Journal Title
Glass And Ceramics 57 5-6 2000 174 - 177
Sector
Glass Ceramics
Class
GC 675

Request article (free for British Glass members)

Correlation Of Properties Of Composite Materials Based On Siloxane Binder With The Type Of Filler
Glass And Ceramics 57 5-6 2000 174 - 177
GC 675