Correlation Of High Refractive Index And Density In High Refractive Index Glasses

The Lorentz-Lorenz, Gladstone-Dale, and Newton-Drude refractivities were determined for a range of TeO2 binary and ternary glasses and also for some soda-lime-silica glasses

Author
S K J Al-Ani, C A Hogarth
Origin
Unknown
Journal Title
J Mater Sci Let 1987 6 5 519-521
Sector
Refractive Indexes
Class
RI 46

Request article (free for British Glass members)