Correlation Between Radiative Transition Probabilities Of Nd3+ And Composition In Silicate, Borate And Phosphate Glasses

Compositional dependence of spontaneous emission probabilities between initial 4F3/2 and terminal 4Ij(J = 9/2, 11/2, 13/2, 15/2) levels of Nd3+ were studied for about 90 samples of silicate, borate, and phosphate glasses using the Judd-Ofelt theory.