Correlation Between Polishing Pad'S Properties And Material Removal During Full-Aperture Polishing

Polishing pad plays a vital role in the fabrication of large flat optical elements during full-aperture polishing. Material removal rate (MRR) and material removal distribution (MRD) describe the material removal process from the point of the global average removal rate and the spatial distribution of removed material, respectively. The pad's mechanical property characterized by compression modulus and morphological characteristic indicated by material ratio curve are used to qualitatively clarify the degression of MRR at different rough polishing stage. Moreover, the novel MRD model is proposed to quantitatively correlate the pads mechanical and morphological characteristic with MRD.

Author
L Ren Et Al
Origin
Harbin Inst Technology, China
Journal Title
Applied Glass Science 10 3 July 2019 287-301
Sector
Flat glass
Class
F 4167

Request article (free for British Glass members)

Correlation Between Polishing Pad'S Properties And Material Removal During Full-Aperture Polishing
Applied Glass Science 10 3 July 2019 287-301
F 4167
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.