Convection Currents In Glass Tanks: Iii, Elementary Theory Of The Motions Of Convection

The mathematical derivation of relations between currents, gradients and dimensions in idealised containers leads to certain rules: (a) the maximum speed of currents in spouts and surface currents in single containers is proportional to the temperature gradient and the cube of the height of spout and tank, respectively. b) The transport of thermal energy is proportional to these. In real tanks a vertical temperature gradient and the ensuing differences in viscosity must be considered. Qualitatively, this consideration leads to the concept of a stagnant layer on the bottom of the tank and a smaller "efficient depth." The neutral zone between current and counter current, ideally placed at six tenths of the depth from the bottom, is placed higher in the real case.

Author
I Peyches
Origin
Unknown
Journal Title
Verres Et Refractaires Aug 1947 26-27
Sector
Primary Papers
Class
PP 134

Request article (free for British Glass members)

Convection Currents In Glass Tanks: Iii, Elementary Theory Of The Motions Of Convection
Verres Et Refractaires Aug 1947 26-27
PP 134
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.