Controlling The Thermal Regime Of Liquid Glass Feeders With Gas Fuel

A new digital system for controlling the thermal regime of a feeder operating on gas fuel and a modified gas-mixing unit giving a mixture with a specified composition in the entire range of fuel flow rates are presented.

Author
B P Shevchenko Et Al
Origin
Khrustal Research Centre, Russia
Journal Title
Glass & Ceramics 53 3-4 102-103