Controlling Glass Furnace Nox With Gas Reburn

Data was used to design modifications to reduce NOx emissions of a large, side-port regenerative container glass furnace.

Author
R Koppang Et Al
Origin
Energy & Environmental Research Corp, Irvine, Calif, Usa
Journal Title
Am Ceram Soc Bull 77 2 1998 51-56
Sector
Container glass
Class
C 1138